Bottle oven

From Infogalactic: the planetary knowledge core
Jump to: navigation, search
Bottle oven, Minkstone Works, Longton (listed building 1220876).

A bottle kiln, or bottle oven, is a type of kiln. The word 'bottle' refers to the shape of the structure and not to the kiln's products, which are pottery, not glass.

Bottle kilns were typical of the industrial landscape of Stoke-on-Trent, where nearly 50 are preserved as listed buildings.[1] Their association with Stoke-on-Trent reflects the fact that the British ceramic industry was mainly based in that city. Bottle kilns are found in other locations; for example Coalport, which had a pottery industry.

Bottle kilns were constructed until the mid-twentieth century after which they were replaced by other types of kiln, as the industry ceased to be coal-fired.

Exterior of bottle ovens at the Gladstone Pottery Museum that was formerly a pot-bank in Longton, Staffordshire (listed building 1195854).

Description

A bottle oven kiln is protected by an outer hovel which helps to create an updraught. The biscuit kiln was filled with saggars of green flatwares (bedded in flint) by placers. The doors (clammins) were bricked up and then the firing began. Each firing took 14 tons of coal. Fires were lit in the firemouths and baited every four hours. Flames rose up inside the kiln and heat passed between the bungs of saggars. They controlled the temperature of the firing using dampers in the crown. The firing was monitored by Bullers rings placed in the kiln. A kiln would be fired to 1250C.[2]

The biscuitwares were glazed and fired again in the bigger glost kilns - again they were placed in saggars, separated by kiln furniture such as stints, saddles and thimbles.

The enamel kiln (or muffle kiln) is of a different construction, with external flues, and was fired at 700C. The pots were stacked on seven or eight levels of clay bats (shelves). The door is iron lined with brick.

Construction

Looking at the kiln from inside the hovel

The brick walls of the inner kiln are around 12 in (300 mm) thick. Around it are iron straps called "bonts". The chamber of the kiln is round with a high domed roof. The floor is also slightly domed, with a central well-hole, while around the walls there are a number of brick bags (chimneys). The kiln was heated from below by a number of coal fires which were stoked from exterior firemouths: the flues from the firemouths pass under the floor to the well-hole and in doing so heated the floor and the kiln. Directly above the firemouths, inside the kiln, are the bags which provided additional chimneys and distributed the direct heat from the flames, up the walls. The height and the diameter of the kiln can vary, and consequently, so did the number of fire mouths. The kiln is entered through a clammin which was designed to be big enough to let in a placer carrying a saggar. The kilns are enclosed in a brick hovel which can be free standing or be part of the work-shop.[3]

Kiln floor, the well-hole and bags

Saggars

<templatestyles src="Module:Hatnote/styles.css"></templatestyles>

Each pot bank made its own saggars from fire clay. In the saggar maker's workshop, clay would be rolled around a wooded form by the saggar maker, while a lad would knock the bottom using a mawl and an iron mould. A saggar could be expected to last for around 40 firings after which it had to be replaced.[2] During biscuit firing, tableware cups and bowls were put on a fine layer of flint dust on the bottom of the saggar, while flatware was supported like a sandwich between layers of flint. They had to be stacked carefully to prevent distortion during firing. Then the saggar was topped and sealed to prevent any fumes or kiln debris entering the saggar and discolouring the wares. During the second firing, the glost firing, the glazed ware was held by pins, saddles, spurs and thimbles, as any contact point would leave a blemish on the glaze.[2] Sorting the thimbles for reuse was one of the lowest jobs in the potbank.[3]

Operation

Bungs of saggars inside the kiln

Placing and drawing the kiln was the job of placers. Placers would take the unfired greenware that was drying in the greenhouse (or the glost placing shop) and stack it in the saggar. They would seal the saggar, then carry it into the bottle oven on their heads. Each loaded saggar weighed around 56 lb (25 kg). They were stacked in bungs in such a way so the most delicate wares were protected. A bung of saggars would be 12 or 13 high, on the top of the bung would be unfired newly moulded green saggars. In the centre of the bottle oven is the well-hole, over it, saggars with no bottoms would be placed in the pipe-bung: this formed a chimney to draw the fires. When the kiln was full, the clammins were bricked up leaving one brick short to form a spyhole so the firemen could watch the buller's rings to judge the temperature of the firing.

The potbank employed a cod placer to supervise the work, but placers who were paid by the job used to wait outside the potbanks for work. Drawing would be done 48 hours after firing finished but in hard times placers were sent into a kiln that was still glowing red after 24. The men wore five layers of clothing and wet cloths over their heads. Life expectancy for a placer was low.[3]

The clammin bricked up ready for firing

A bottle oven would be fired once a week. The fires were set in each of the firemouths by the firemen. Once alight the kiln would be heated slowly as the moisture was burned out of the clay, this was known as "smoking". Then the kiln would be taken to full temperature, and kept there for three hours then allowed to cool. A biscuit firing took three days and a glost firing took two days.[3] After 48 hours the kiln had cooled sufficiently to be drawn by the placers, and the wares checked. The placers' earnings were dependent on the success of the firing.

Each firing would use 14 tons (13 tonnes) of coal. It was very energy inefficient and popular sources[3] say that between 50% and 95% of the heat was lost up the chimney. Coal burning is a very dirty process; the smoke from a bottle kiln would eddy around the kiln top, and curl down to ground level either into the yard of the pot bank or into the streets and houses around.[3]

A firemouth- in museum conditions

Preservation

There are 47 standing bottle ovens in Stoke-on-Trent, all are now listed buildings. Bottle ovens can be seen at the Gladstone Pottery Museum, Burleigh Pottery and the Ironbridge Gorge Museum.

References

  1. Lua error in package.lua at line 80: module 'strict' not found.